Description

HP2023JN is a Low Density Polyethylene grade suitable for general-purpose packaging. They exhibit better draw down, good optical and mechanical properties. HP2023JN contains slip and antiblock additives.
 

TYPICAL APPLICATIONS

Thin shrink film, lamination film, produce bags, textile packaging, soft goods packaging, general-purpose bags with good optics and t-shirts carrier bags.
 

Properties

PROPERTIES TYPICAL VALUES UNITS     TEST METHODS
POLYMER PROPERTIES      
Melt Flow Rate      
at 190°C and 2.16 kg 2 g/10 min ASTM D1238
Density      
at 23°C 923 kg/m³ ASTM D1505
FORMULATION      
Slip agent   - -
Anti block agent   - -
MECHANICAL PROPERTIES      
Dart Impact Strength 2 g/µm ASTM D1709
OPTICAL PROPERTIES      
Haze (1) 8 % ASTM D1003
Gloss      
at 45° 61 - ASTM D2457
FILM PROPERTIES      
Tensile Properties      
stress at break, MD 20 MPa ASTM D882
stress at break, TD 15 MPa ASTM D882
strain at break, MD 300 % ASTM D882
strain at break, TD 588 % ASTM D882
stress at yield, MD 12 MPa ASTM D882
stress at yield, TD 12 MPa ASTM D882
1% secant modulus, MD 235 MPa ASTM D882
1% secant modulus, TD 271 MPa ASTM D882

 

 

PROCESSING CONDITIONS

Typical processing conditions for HP2023JN are:
Barrel temperature: 160 - 190°C
Blow up ratio: 2.0 - 3.0
 

HEALTH, SAFETY AND FOOD CONTACT REGULATIONS

Detailed information is provided in the relevant Material Safety Datasheet and or Standard Food Declaration, Additional specific information can be requested via your local Sales Office.
DISCLAIMER: This product is not intended for and must not be used in any pharmaceutical/medical applications.
 

STORAGE AND HANDLING

Polyethylene resin should be stored in a manner to prevent a direct exposure to sunlight and/or heat. The storage area should also be dry and preferably do not exceed 50°C. SABIC would not give warranty to bad storage conditions which may lead to quality deterioration such as color change, bad smell and inadequate product performance. It is advisable to process PE resin within 6 months after delivery
 